Test Data: PRO-POXY 204
ASTM C-881 | Types I, II, IV & V | Grade 2, Classes B & C
Download PDF (19 Kb PDF)

 

           LABORATORY TESTS

   RESULTS

           SPECIFICATIONS

D-2393  Viscosity 

6,000 cps  

2000 cps - 10,000 cps

C-881   Gel Time

15 minutes

 

C-882   Bond Strength (2 day cure)

3,450 psi

1,000 psi1,4  minimum

C-882   Bond Strength (14 day cure)

4,800 psi

1,500 psi1,2,4,5 minimum

D-695   Compressive Strength

12,823 psi

5,000 psi2

8,000 psi1,5

10,000 psi4 minimum

D-695   Modulus of Elasticity

226,600 psi

90,000 psi2

150,000 psi1,5

200,000 psi4 minimum

D-638   Tensile Strength

7,280 psi

2,000 psi2

5,000 psi1

6,000 psi5

7,000 psi4 minimum

D-2566  Linear Coefficient of Shrinkage

0.0016

0.0051,2,4,5 maximum

D-638   % Elongation at Break

3.8%

1.0%1,2,4,5 minimum

D-570   Absorption

0.61%

1.0%1,2,4,5 maximum

D-648   Heat Deflection Temp

125กใF

120กใF4,5  minimum

D-2240  Shore D Hardness

85

N/A

   1 - Type I

   2 - Type II

   4 - Type IV

   5 - Type V

 
  ©2000-2005 Unitex | mail@unitex-chemicals.com | Internet Disclaimer | Warranty Disclaimer