LABORATORY TESTS
|
RESULTS
|
ASTM C-881 SPECIFICATIONS
|
|
Mix Ratio (A to B by volume)
|
10 to 1
|
n/a
|
|
C-881 Consistency
|
0 (no flow)
|
¼” flow maximum4
|
|
C-881 Gel
Time
|
7.5 minutes
|
5 minutes minimum4
|
|
D-695 Compressive
Strength
|
10,540 psi
|
10,000 psi minimum4
|
|
D-695 Compressive
Modulus
|
265,000 psi
|
200,000 psi minimum4
|
|
D-570 Absorption
|
0.08%
|
1% maximum4
|
|
D-648 Heat
Deflection Temperature
|
144°F
|
120°F minimum4
|
|
C-882 Bond
Strength (2 day)
|
2,890 psi
|
1000 psi minimum4
|
|
C-882 Bond
Strength (14 day)
|
3,250 psi
|
1500 psi minimum4
|
|
D-2566 Linear Coefficient of Shrinkage
|
0.005
|
0.005 maximum
|
|
D-638 Elongation
at Break
|
1.321%
|
1% minimum4
|
|
D-1875 Density
(lb/gal) Component A
|
12.92
|
n/a
|
|
D-1875 Density
(lb/gal) Component B
|
13.69
|
n/a
|
4
- ASTM C-881, Type IV – load bearing specifications
* -
Consult Unitex for details and instructions
|
|
 |